CYC Specification for Strotium wet pressing Magnetic Materials:
CYC Brand Series Strontium Ferrite Magnetic Powders have been designed to produce all grades of hard ferrites. The users will make high quality magnets by adding the provided additives into the powders. Our highly automatic instruments and strict quality control system ensure that the quality is stable and reliable.
TIPY
|
Br
|
Hcb
|
Hcj
|
(BH)max
|
|
%
|
TRAD
|
mT
|
Gs
|
kA/m
|
Oe
|
kA/m
|
Oe
|
kJ/m³
|
MGOe
|
(g/cm³)
|
〦
|
CYC29
|
370
|
3700
|
270
|
3390
|
318
|
4000
|
26.1
|
3.28
|
4.8
|
13+/-0.5
|
CYC30
|
390
|
3900
|
231
|
2900
|
235
|
2950
|
28.7
|
3.60
|
4.8
|
13+/-0.5
|
CYC30B
|
410
|
4100
|
200
|
2510
|
207
|
2600
|
31.2
|
3.90
|
4.8
|
13+/-0.5
|
CYC29H
|
360
|
3600
|
271
|
3400
|
382
|
4800
|
24.0
|
3.01
|
4.8
|
13+/-0.5
|
CYC31
|
410
|
4100
|
231
|
2900
|
235
|
2950
|
32.6
|
4.09
|
4.9
|
13+/-0.5
|
CYC32
|
380
|
3800
|
279
|
3500
|
318
|
4000
|
26.2
|
3.29
|
4.8
|
13+/-0.5
|
CYC33
|
400
|
4000
|
267
|
3350
|
279
|
3500
|
30.3
|
3.80
|
4.9
|
13+/-0.5
|
CYC34
|
420
|
4200
|
223
|
2800
|
227
|
2850
|
33.6
|
4.20
|
4.9
|
13+/-0.5
|
CYC35
|
400
|
4000
|
290
|
3640
|
318
|
4000
|
31.2
|
3.90
|
4.9
|
13+/-0.5
|
CYC35B
|
420
|
4200
|
255
|
3200
|
263
|
3300
|
34.4
|
4.30
|
4.9
|
13+/-0.5
|
CYC36
|
410
|
4100
|
300
|
3770
|
350
|
4400
|
32.8
|
4.10
|
4.9
|
11.5+/-0.5
|
CYC36B
|
425
|
4250
|
290
|
3640
|
318
|
4000
|
35.2
|
4.40
|
4.9
|
11.5+/-0.5
|
CYC36H
|
390
|
3900
|
302
|
3790
|
382
|
4800
|
28.9
|
3.60
|
4.9
|
11.5+/-0.5
|
CYC37H
|
420
|
4200
|
318
|
4000
|
382
|
4800
|
34.4
|
4.30
|
4.9
|
11.5+/-0.5
|
CYC37B
|
440
|
4400
|
318
|
4000
|
350
|
4400
|
36.7
|
4.6
|